MODIFIED BITUMEN ROOFS

Restoring a modified bitumen roof: pull tests, seams and building to thickness

A modified bitumen roof that is secured to the deck, sits on dry insulation and passes an adhesion pull test can be restored with a reinforced, liquid-applied restoration system instead of being torn off. Most of the job is preparation: moisture survey, repairs, seam detailing and pull tests all come before the first coat.

Prepared by NanoGuard SolutionsLast reviewed ·
At least 3 in.above flashingsReinforced restorationsystem, built towarranty thicknessRecover board, seamssealed (where specified)Existing modified bitumen:repaired and pull-testedInsulation: dry, confirmedby moisture surveyRoof deck
Diagram · A modified bitumen restoration, from the deck up.

What has to be true before work starts

The existing membrane needs reasonable surface integrity and has to be fastened down to the roof deck. A moisture survey, using a method the manufacturer approves, is done before anything is installed, and every wet area it finds is removed; the insulation underneath has to remain dimensionally sound.

Ponding is fixed first: drainage deficiencies are corrected before the system goes on. Where too much of the roof has failed, the restore-or-replace guide covers the call.

Adhesion pull tests decide whether it goes ahead

Pull tests are spread evenly across the roof, and the number is set for each job. They are taken only after the required dry time.

If a test fails, a primer goes on and the test is run again. If it fails twice, the roof is not coated.

Aluminized asphalt and asphalt mastic are removed as far as possible, and those patches may need pull tests of their own.

Cleaning, repairs and seams

What the prep covers
What is foundWhat is done
Equipment and conduit that no longer serve the buildingTaken off the roof.
Loose gravel and debrisCleared with a power broom or blower.
Loose exposed fasteners, seams or lapsFasteners tightened, with extra fasteners sunk where seams or laps have worked loose.
Fish mouths, wrinkles and voidsRepaired to industry standards before the system goes on.
Penetrations such as pitch pans and pipe bootsInstalled to industry standards first.
SeamsSealed with a 6-inch band of fibre-reinforced seam sealer, or three-coursed with fabric and sealant, then cured overnight and inspected.
Rusted galvanized or bare metalWire-brushed, then primed against rust.

Where the specification calls for a recover board, a ½-inch board is installed over the cleaned roof to building-code and wind-uplift requirements, and its seams are sealed before coating.

Building the system to thickness

The system goes onto a clean, dry surface and runs at least 3 inches above every flashing, repair, parapet and equipment base, with extra attention at seams and repaired areas. Each coat dries and is inspected before the next one.

Film thickness follows the warranty term; the dry film for each term is on the warranty page.

Weather limits in the specification: no work below 45°F (7°C), above 85% relative humidity or within 4 hours of sundown, and the surface must be free of dew before starting and between coats. Nothing goes onto a wet, dirty or frozen roof.

Inspection and warranty conditions

A roof plan is required, and the final inspection is called within 7 days of finishing. For the manufacturer warranty, the installer must hold Approved Applicator status, the roof must meet the square-foot minimum, and the finished membrane must be continuous and meet the minimum thickness.

Your next step

Tell us the building, the roof's approximate area and where it leaks or holds water. Our free visual review walks the membrane, seams and drainage; where moisture needs confirming, a paid full condition assessment follows, as the commercial roof assessment guide explains.

Questions

Can a modified bitumen roof with loose gravel be restored?

Yes, if the membrane underneath qualifies. Loose gravel is cleared off first, and where the specification calls for a recover board, it goes down before the system.

What happens if the coating won't stick to the old membrane?

A primer is applied and the pull test is repeated over it. A second failure rules that roof out for this system.

How thick does the system go on a mod-bit roof?

It depends on the warranty term: from 23 mils dry for 10 years to 52 mils dry for 20. An irregular or porous membrane can need extra material to reach that film.

Book a roof assessmentCall